Started the day by putting the two pocket pieces into place with one ply of BID on each side of the foam piece.
This took a while as I was running low on hardener and needed to boil some water so I could get what I had back to a liquid state. The hardener goes solid in the glass jars I store it in, so you have to heat it in order for it to return to a liquid state. I also needed to put in some more resin into the pump container as it too was low. Then it was just a matter of wetting out the fiberglass and covering the foam with Micro Slurry and put everything into place followed by some peel ply to make it nice and smooth.

11/25/2013   Picture 418